Saturday, July 19, 2014
Waterjetting 23c - Abrasive Slurry cutting range
In an early section of these notes on high-pressure water and its uses, there was a review of some of the ways in which jet power could be assessed. For the most part the best way to see how changes in a system alter the way the jets cut is to run a simple cutting test and in many cases it will give the answer that is needed. However, sometimes it is important to go beyond the simple assessment of whether condition (a) is better than condition (b) and to try and explain why it is.
One of the early discoveries in trying to explain abrasive jet behavior was made by my colleagues Marian Mazurkiewicz and Greg Galecki who showed that, when creating an abrasive waterjet system in the conventional way, that a large amount of the abrasive was being fragmented in the mixing chamber of the nozzle.
Figure 1. Size distribution of garnet particles after being fed through the mixing chamber of an abrasive waterjet nozzle, AFR 0.6 lb/min, at 30,000 psi.
Before entering the chamber the particles had been screened to be very close to an average 200 micron size. After going through the chamber the average particle size (50%) was 140 microns, with roughly 25% of the particles being smaller than 100 microns, at which point we had found that the cutting performance gets significantly poorer.
The way in which we found the particle size, (and also assessed how fast the particles were moving after they left the nozzle) was to set the nozzle horizontally, and then to fire the jet down the center of a large plastic tube.
Figure 2. Plastic tube set up to capture the abrasive particles from an abrasive waterjet nozzle. (The nozzle is on the left of the tube).
Barriers were placed at 1-ft intervals along the tube, so that as the particles lost energy and fell to the bottom of the pipe they could be collected into the small dark blue containers under the tube, and then dried, sized and weighed. During a test the top half of the pipe sections are replaced, so that the jet is contained over the pipe length, which was just over 20-ft, and this was long enough to capture, within the length, all the abrasives from all the tests of abrasive waterjet nozzles that we carried out (which included all those commercially available at the time).
It was based in part on this test that we were able to understand why some abrasive waterjet nozzle designs work better than others, and also to begin to understand more of the mechanisms that drive the cutting process.
As the abrasive slurry system (ASJ) started to enter the American market we were thus ready to test the way in which it worked and to see if we could find any improvement, as had been reported by those who first used the system.
When we set the system up so that the ASJ system fed a nozzle in the same arrangement as with the AWJ system we got a surprise. Much of the abrasive was collecting at the far end of the pipe, and it was starting to poke a hole through the end piece.
Over time we extended the tube, and eventually moved it outside to ensure that we could capture all the abrasive in the same way as earlier.
Figure 3. The test set-up needed to capture all the abrasive when using an abrasive slurry jet rather than an abrasive waterjet. (The pipe is roughly 50-ft long).
Even at lower pressures the ASJ was carrying the abrasive much further than was the case with the conventional AWJ system, showing that the particles were retaining more energy over greater distances. In retrospect this is not surprising, since there is sensibly no break-up of the abrasive particles with the ASJ system during the mixing and acceleration of the particles.
This is because the particles are mixed in with the water before the water accelerates, and when it does the abrasive is already mixed throughout the jet, rather than trying to force its way into the jet, while at relatively slow velocity relative to the water. There is, as a result, no break-up of the particles, and larger particles will lose energy more slowly than smaller ones. (One of the findings of the AWJ tests carried out earlier).
In addition because there is no air in the ASJ jet stream there is no active component trying to disrupt the jet, and as a result the water remains coherent to a greater distance from the nozzle, and has, as a result, a much greater capability of transferring the energy to the particles to accelerate them to their full potential, given the design of the system.
There are various different ways in which this benefit can be illustrated, using lab data, but the clearest demonstration is to take a conventional waterjet system, and to run the triangle test and then, with the same amount of abrasive in the jet stream, and a roughly equivalent amount of water, to run the same test with an abrasive slurry system.
Figure 4. Comparison of the cuts achieved with an abrasive slurry system (upper) and an abrasive waterjet system (lower).
The picture shows that the two systems are cutting to sensibly the same depth, and the ASJ system is being operated at a quarter of the pressure of the equivalent AWJ system.
There have been many comparisons between the two systems in the time since this initial evaluation was made, and there is a rough consistency in the results that have been obtained, on the order of that shown in figure 4. The comparisons are not all equivalent to this, since the tests compare different attributes of the two systems, and, for example, there are additional advantages of the lower pressure ASJ system that can enhance the relative performance. One way, when one compares equivalent horsepower, is to increase the diameter of the ASJ nozzle. This allows use of a larger abrasive particle that, in turn, will give a further increase in achievable depth of cut.
Unfortunately the difficulties in achieving consistent performance with some ASJ systems, over long operating periods, has made it more difficult for this relatively new system to penetrate fully into the market place as yet.
One of the early discoveries in trying to explain abrasive jet behavior was made by my colleagues Marian Mazurkiewicz and Greg Galecki who showed that, when creating an abrasive waterjet system in the conventional way, that a large amount of the abrasive was being fragmented in the mixing chamber of the nozzle.
Figure 1. Size distribution of garnet particles after being fed through the mixing chamber of an abrasive waterjet nozzle, AFR 0.6 lb/min, at 30,000 psi.
Before entering the chamber the particles had been screened to be very close to an average 200 micron size. After going through the chamber the average particle size (50%) was 140 microns, with roughly 25% of the particles being smaller than 100 microns, at which point we had found that the cutting performance gets significantly poorer.
The way in which we found the particle size, (and also assessed how fast the particles were moving after they left the nozzle) was to set the nozzle horizontally, and then to fire the jet down the center of a large plastic tube.
Figure 2. Plastic tube set up to capture the abrasive particles from an abrasive waterjet nozzle. (The nozzle is on the left of the tube).
Barriers were placed at 1-ft intervals along the tube, so that as the particles lost energy and fell to the bottom of the pipe they could be collected into the small dark blue containers under the tube, and then dried, sized and weighed. During a test the top half of the pipe sections are replaced, so that the jet is contained over the pipe length, which was just over 20-ft, and this was long enough to capture, within the length, all the abrasives from all the tests of abrasive waterjet nozzles that we carried out (which included all those commercially available at the time).
It was based in part on this test that we were able to understand why some abrasive waterjet nozzle designs work better than others, and also to begin to understand more of the mechanisms that drive the cutting process.
As the abrasive slurry system (ASJ) started to enter the American market we were thus ready to test the way in which it worked and to see if we could find any improvement, as had been reported by those who first used the system.
When we set the system up so that the ASJ system fed a nozzle in the same arrangement as with the AWJ system we got a surprise. Much of the abrasive was collecting at the far end of the pipe, and it was starting to poke a hole through the end piece.
Over time we extended the tube, and eventually moved it outside to ensure that we could capture all the abrasive in the same way as earlier.
Figure 3. The test set-up needed to capture all the abrasive when using an abrasive slurry jet rather than an abrasive waterjet. (The pipe is roughly 50-ft long).
Even at lower pressures the ASJ was carrying the abrasive much further than was the case with the conventional AWJ system, showing that the particles were retaining more energy over greater distances. In retrospect this is not surprising, since there is sensibly no break-up of the abrasive particles with the ASJ system during the mixing and acceleration of the particles.
This is because the particles are mixed in with the water before the water accelerates, and when it does the abrasive is already mixed throughout the jet, rather than trying to force its way into the jet, while at relatively slow velocity relative to the water. There is, as a result, no break-up of the particles, and larger particles will lose energy more slowly than smaller ones. (One of the findings of the AWJ tests carried out earlier).
In addition because there is no air in the ASJ jet stream there is no active component trying to disrupt the jet, and as a result the water remains coherent to a greater distance from the nozzle, and has, as a result, a much greater capability of transferring the energy to the particles to accelerate them to their full potential, given the design of the system.
There are various different ways in which this benefit can be illustrated, using lab data, but the clearest demonstration is to take a conventional waterjet system, and to run the triangle test and then, with the same amount of abrasive in the jet stream, and a roughly equivalent amount of water, to run the same test with an abrasive slurry system.
Figure 4. Comparison of the cuts achieved with an abrasive slurry system (upper) and an abrasive waterjet system (lower).
The picture shows that the two systems are cutting to sensibly the same depth, and the ASJ system is being operated at a quarter of the pressure of the equivalent AWJ system.
There have been many comparisons between the two systems in the time since this initial evaluation was made, and there is a rough consistency in the results that have been obtained, on the order of that shown in figure 4. The comparisons are not all equivalent to this, since the tests compare different attributes of the two systems, and, for example, there are additional advantages of the lower pressure ASJ system that can enhance the relative performance. One way, when one compares equivalent horsepower, is to increase the diameter of the ASJ nozzle. This allows use of a larger abrasive particle that, in turn, will give a further increase in achievable depth of cut.
Unfortunately the difficulties in achieving consistent performance with some ASJ systems, over long operating periods, has made it more difficult for this relatively new system to penetrate fully into the market place as yet.
Read more!
Tuesday, December 10, 2013
Waterjetting 16b - Optimum Abrasive Feed Rate and Depth
The post that I wrote last week was focused on the misperception that you need to add more abrasive to an abrasive waterjet if you wish to cut through thicker material. This is wrong on a number of counts, but most particularly because a good operator will have tuned the nozzle to achieve the best cutting jet, based on pressure and abrasive feed rate (AFR) regardless of target material. What the operator may change is the operating pressure (which would change the optimum AFR) and the traverse speed since these control the depth and quality of the cut that the jet makes.
But, before leaving the topic, I would like to discuss, in a little more detail, the concept of the optimal amount of abrasive that one should use with a given jet, and what happens as that feed rate is changed. As I mentioned last time, because of differences in the shapes of the mixing chambers of the nozzles supplied by different manufacturers, the specific sizes and optimal flow rates will differ from nozzle to nozzle but the overall conclusions remain the same.
Last time I pointed out that the driving waterjet had to break up within the mixing chamber in order to properly mix with the abrasive and to bring this up to a maximum speed before the mix left the focusing tube. Where the driving jet is too large then this breakup is not complete and the mixing is not efficient. As a result the jet that comes out of the end is more diffuse and the abrasive will not have reached the full velocity possible. However, if the incoming waterjet is made smaller for the same AFR and other mixing chamber geometries, then the cutting performance will decline.
Figure 1. Effect of increase in jet pressure when cutting aluminum with an AFR of 1.7 lb/minute (after Hashish, M., "Abrasive Jets," Section 4, in Fluid Jet Technology- Fundamentals and Applications, Waterjet Technology Association, St. Louis, MO, 1991.)
For a similar reason adding a polymer to the jet fluid should only be carried out with some care for the consequences. Long-chain polymers can give a jet increased cohesion and this can, at high enough concentrations, inhibit jet breakup in the mixing chamber thus reducing the effectiveness of mixing in the chamber.
Figure 2. The effect of changing cutting fluid on AWJ performance (after Dr Hashish ibid)
Polyox, (polyethylene oxide) is an extremely effective polymer for increasing jet performance by cohering the jet and reducing the friction losses between the pump and the nozzle. However, as the graph shows, adding it to some abrasive systems will reduce performance since the more coherent jet makes it more difficult for the abrasive to mix and accelerate to full velocity. At lower concentrations the polymer allows the jet to breakup, but keeps the slugs of water together making energy transfer more efficient. Higher velocity abrasive means that less is required to achieve the same cutting performance as Walters and Saunders showed.
Figure 3. Effect of adding polymer in reducing the amount of abrasive required to cut stainless steel (after Walters, C.L., Saunders, D.H., "DIAJET Cutting for Nuclear Decommissioning," Paper J2, 10th International Symposium on Jet Cutting Technology, Amsterdam, Netherlands, October, 1990, pp. 427 - 440.)
At low levels of abrasive feed Dr Hashish has shown that increasing the amount of abrasive in the feed increases cutting performance.
Figure 4. Effect of increase in AFR on depth of cut in mild steel at a feed rate of 6 inches/min (After Dr. Hashish ibid), waterjet diameter 0.01 inches.
However, as the abrasive flow rate continues to increase the cutting performance reaches a plateau and can decline, as Dr. Hashish illustrated. An AFR of 20 gm/sec is equivalent to a feed of 2.6 lb/minute.
Figure 5. The effect of higher AFR on cutting depth at 3 jet pressures on a mild steel target (after Dr. Hashish ibid)
Note that in this case the nozzle geometry was not optimized for operation at the highest jet pressure. More visibly we ran a series of cuts across a granite sample, where the only thing that changed between cuts was that we increased the abrasive feed rate in cuts from the left to the right. It can be seen that beyond a certain AFR the jet starts to cut to a shallower depth.
Figure 6. Successive cuts made into a granite block at increasing AFR from the left to the right.
Interestingly the optimum feed rate doesn’t just depend on the pressure and water flow rate (waterjet orifice size) of the system. Faber and Oweinah have shown that as the feed particle size gets larger, so the optimum AFR reduces.
Figure 7. Optimal Abrasive feed rate as a function of particle size (after Faber, K., Oweinah, H., "Influence of Process Parameters on Blasting Performance with the Abrasive Jet," paper 25, 10th International Symposium on Jet Cutting Technology, Amsterdam, October, 1990, pp. 365 - 384.)
The process of finding an optimal feed rate for a system is thus controlled by the design of the mixing chamber based on the relative position of the abrasive feed tube and the size of the waterjet orifice. This controls how well the abrasive that is fed into the system can mix with the jet and acquire the velocity that it needs for most effective cutting. Then, as the above plot shows, the optimal AFR is also influenced by the size of the particles that are being fed into the system, since as the particles become larger beyond a certain size, so the cutting effectiveness declines.
Part of the reason for this is that, as the AFR increases so there is an increased risk of particle to particle impact breaking the particles down into smaller sizes. (And an earlier post showed that smaller particles cut less effectively – as does figure 7 above). We screened the particles that came from several different designs of AWJ nozzle assemblies capturing them after they left the nozzle but without further impact, so that the size range is indicative of that which a target material would see,
The table is a summary of some of the results and it shows results for a feed that began at 250 microns giving the percentage of the particles that survived at larger than 100 microns.
Figure 8. Percentage of the 250 micron sized feed that survives at above 100 micron for differing jet conditions. (the numbers are averaged from several tests).
It can be seen that when the feed rate rises to 1.5 lb a minute that there is a drop in abrasive size at higher jet pressures, and this is likely to be due to the increased interaction with particles. Since cutting effectiveness is controlled by particle size, count and velocity the only slightly greater amount of particles that survive above 100 microns at 1.5 lb/minute relative to those that survive at 1 lb/minute suggest that spending the money to increase the AFR above the optimal value (in this case around 1 lb/min) is a wasted investment.
It is therefore important to tune the system to ensure that, for each jet pressure and nozzle design that is used, that the AFR has been optimized.
But, before leaving the topic, I would like to discuss, in a little more detail, the concept of the optimal amount of abrasive that one should use with a given jet, and what happens as that feed rate is changed. As I mentioned last time, because of differences in the shapes of the mixing chambers of the nozzles supplied by different manufacturers, the specific sizes and optimal flow rates will differ from nozzle to nozzle but the overall conclusions remain the same.
Last time I pointed out that the driving waterjet had to break up within the mixing chamber in order to properly mix with the abrasive and to bring this up to a maximum speed before the mix left the focusing tube. Where the driving jet is too large then this breakup is not complete and the mixing is not efficient. As a result the jet that comes out of the end is more diffuse and the abrasive will not have reached the full velocity possible. However, if the incoming waterjet is made smaller for the same AFR and other mixing chamber geometries, then the cutting performance will decline.
Figure 1. Effect of increase in jet pressure when cutting aluminum with an AFR of 1.7 lb/minute (after Hashish, M., "Abrasive Jets," Section 4, in Fluid Jet Technology- Fundamentals and Applications, Waterjet Technology Association, St. Louis, MO, 1991.)
For a similar reason adding a polymer to the jet fluid should only be carried out with some care for the consequences. Long-chain polymers can give a jet increased cohesion and this can, at high enough concentrations, inhibit jet breakup in the mixing chamber thus reducing the effectiveness of mixing in the chamber.
Figure 2. The effect of changing cutting fluid on AWJ performance (after Dr Hashish ibid)
Polyox, (polyethylene oxide) is an extremely effective polymer for increasing jet performance by cohering the jet and reducing the friction losses between the pump and the nozzle. However, as the graph shows, adding it to some abrasive systems will reduce performance since the more coherent jet makes it more difficult for the abrasive to mix and accelerate to full velocity. At lower concentrations the polymer allows the jet to breakup, but keeps the slugs of water together making energy transfer more efficient. Higher velocity abrasive means that less is required to achieve the same cutting performance as Walters and Saunders showed.
Figure 3. Effect of adding polymer in reducing the amount of abrasive required to cut stainless steel (after Walters, C.L., Saunders, D.H., "DIAJET Cutting for Nuclear Decommissioning," Paper J2, 10th International Symposium on Jet Cutting Technology, Amsterdam, Netherlands, October, 1990, pp. 427 - 440.)
At low levels of abrasive feed Dr Hashish has shown that increasing the amount of abrasive in the feed increases cutting performance.
Figure 4. Effect of increase in AFR on depth of cut in mild steel at a feed rate of 6 inches/min (After Dr. Hashish ibid), waterjet diameter 0.01 inches.
However, as the abrasive flow rate continues to increase the cutting performance reaches a plateau and can decline, as Dr. Hashish illustrated. An AFR of 20 gm/sec is equivalent to a feed of 2.6 lb/minute.
Figure 5. The effect of higher AFR on cutting depth at 3 jet pressures on a mild steel target (after Dr. Hashish ibid)
Note that in this case the nozzle geometry was not optimized for operation at the highest jet pressure. More visibly we ran a series of cuts across a granite sample, where the only thing that changed between cuts was that we increased the abrasive feed rate in cuts from the left to the right. It can be seen that beyond a certain AFR the jet starts to cut to a shallower depth.
Figure 6. Successive cuts made into a granite block at increasing AFR from the left to the right.
Interestingly the optimum feed rate doesn’t just depend on the pressure and water flow rate (waterjet orifice size) of the system. Faber and Oweinah have shown that as the feed particle size gets larger, so the optimum AFR reduces.
Figure 7. Optimal Abrasive feed rate as a function of particle size (after Faber, K., Oweinah, H., "Influence of Process Parameters on Blasting Performance with the Abrasive Jet," paper 25, 10th International Symposium on Jet Cutting Technology, Amsterdam, October, 1990, pp. 365 - 384.)
The process of finding an optimal feed rate for a system is thus controlled by the design of the mixing chamber based on the relative position of the abrasive feed tube and the size of the waterjet orifice. This controls how well the abrasive that is fed into the system can mix with the jet and acquire the velocity that it needs for most effective cutting. Then, as the above plot shows, the optimal AFR is also influenced by the size of the particles that are being fed into the system, since as the particles become larger beyond a certain size, so the cutting effectiveness declines.
Part of the reason for this is that, as the AFR increases so there is an increased risk of particle to particle impact breaking the particles down into smaller sizes. (And an earlier post showed that smaller particles cut less effectively – as does figure 7 above). We screened the particles that came from several different designs of AWJ nozzle assemblies capturing them after they left the nozzle but without further impact, so that the size range is indicative of that which a target material would see,
The table is a summary of some of the results and it shows results for a feed that began at 250 microns giving the percentage of the particles that survived at larger than 100 microns.
Figure 8. Percentage of the 250 micron sized feed that survives at above 100 micron for differing jet conditions. (the numbers are averaged from several tests).
It can be seen that when the feed rate rises to 1.5 lb a minute that there is a drop in abrasive size at higher jet pressures, and this is likely to be due to the increased interaction with particles. Since cutting effectiveness is controlled by particle size, count and velocity the only slightly greater amount of particles that survive above 100 microns at 1.5 lb/minute relative to those that survive at 1 lb/minute suggest that spending the money to increase the AFR above the optimal value (in this case around 1 lb/min) is a wasted investment.
It is therefore important to tune the system to ensure that, for each jet pressure and nozzle design that is used, that the AFR has been optimized.
Read more!
Friday, December 6, 2013
Waterjetting 16a - Abrasive Feed
I was talking with someone the other day who mentioned that it was necessary to increase the amount of abrasive feed to a waterjet whenever the material to be cut was thicker. This is actually a myth, or put another way, wrong! It is the equivalent of saying that you should use a duller knife if you want to cut thinner material.
Today’s topic therefore is about optimizing the abrasive feed rate into an abrasive waterjet cutting system, but you should remember that different manufacturers have different nozzle assembly designs. Thus the graphs and tables that I will use to illustrate the discussion relate to one particular nozzle design that was used at that time. Not all the nozzle designs were the same, but the results illustrate the points that I am going to make. But it underlies the recommendation that you should each run some standard tests with your system so that you have a baseline of performance and data to tell you where your system works best.
There are several reasons why different designs produce different cutting results, and I will point out some of them in what follows. To begin, however, consider again the basic elements of the waterjet mixing chamber.
Figure 1. Section through the mixing chamber of a conventional abrasive injection system.
A small high pressure stream of water enters the chamber through the upper nozzle, passes through the chamber, creating a vacuum that pulls abrasive into the chamber, and mixes with that abrasive before the resulting AWJ exits through the focusing tube.
One of the first things to understand is that, in the cutting jet that issues from the tube the actual cutting comes from the abrasive particles. From work that has been carried out at a number of places we know that the higher the velocity of the particles, the greater the damage that they will do on the target.
Figure 2. Relative mass loss when steel balls hit a mild steel plate (after Hutchings, I.M., Winter, R.E., Field, J.E., "Solid Particle Erosion of Metals;The Removal of Surface Material by Spherical Projectiles," Proceedings of the Royal Society, London, Vol. A348, 1976, pp. 379 - 392.)
Discussion in earlier posts pointed out that there are different ways in which waterjets attack ductile and brittle materials. However the relationship between an increase in impact velocity and damage occurs whether the targets are brittle or ductile. In figure 2 the target was a ductile steel, in more brittle material it is the coalescence of cracks that removes material, and higher velocities create larger cracks, as shown in figure 3.
Figure 3. Effect of impact velocity on crack length, (after Evans, A.G., "Impact Damage Mechanics: Solid Projectiles," in Erosion, Treatise on Materials Science and Technology, Vol. 16, ed C. Preece, Academic Press, 1979.).
And the same form holds true if steel balls are fired into sandstone.
Figure 4. Relative amount of Berea sandstone removed by the impact of steel balls of varying size (after Ripkin, J.F., Wetzel, J.M., A Study of the Fragmentation of Rock byImpingement with Water and Solid Impactors, Final Report on U.S. Bureau of Mines, Contract HO 210021, February, 1972.).
The above graphs show that it is more effective to have the abrasive moving faster in terms of the damage done by individual particles. Which brings up the first consideration in the design and use of an AWJ mixing chamber.
In order to get the particles moving as fast as possible they have to get their energy from the water jet entering the chamber. But the jet enters the chamber as a solid stream that then breaks into droplets (as shown in earlier pictures) as it passes down the chamber. If the jet remains in a solid stream all the way down, and out of the focusing tube, then the abrasive will find it difficult to penetrate into the center of the jet stream and pick up all the needed jet energy.
This can be illustrated by looking at the velocity and distribution of particles coming out of a nozzle with two different sizes of waterjet orifice but the same size of focusing tube diameter.
Figure 5. Relative particle distribution across a 40,000 psi jet with a focusing tube diameter of 2.3 mm (0.09 inches), and an AFR of 1 lb/min for two waterjet orifice sizes (after Mazurkiewicz, M., Olko, P., Jordan, R., "Abrasive Particle Distribution in a High Pressure Hydroabrasive Jet," International Water Jet Symposium, Beijing, China, September, 1987, pp. 4-1 - 4-10.)
The smaller waterjet breaks up fully within the chamber entraining and accelerating the abrasive particles and providing the desired cutting stream. The larger sized jet does not completely breakup, and fewer particles can mix into the center of the jet giving a more diffuse and less efficient cutting stream. In this case changing from a 0.005 inch waterjet orifice to a 0.013 inch diameter orifice (at roughly 7 times more power, because of the higher flow rate) produces a poorer result.
It is therefore important to ensure that there is an efficient energy transfer between the water and the particles. But the jet energy can only be diffused to a certain number of particles before it significantly begins to reduce in the amount of energy that it imparts to each particle. In other words if you put too much abrasive into the jet stream, then the amount of energy each particle gets is reduced, as it the overall cutting efficiency.
In an example I have used in class I noted that if I pick up a small child and run down the corridor, then I can carry the child at about my normal running speed, on the other hand if I pick up a couple of football players and try the same run I will be barely able to stagger. So the optimum carrying capacity of any jet can be determined for a given water flow rate, which is itself based on the waterjet orifice diameter and the pressure at which the water is supplied.
I will return to this topic next time, but you can see, in the concluding figure, that when a lower abrasive feed rate is fed to the nozzle, that the percentage of the abrasive moving in the higher velocity range rises to over 60% compared with only 20% of the particles when the abrasive feed is too high. And that means that the cutting performance will be less with the higher abrasive feed rates. (The numbers are a little high to reinforce the point).
Figure 7. Particle velocity distribution on leaving the focusing tube (after Isobe, T., Yoshida, H., Nishi, K., "Distribution of Abrasive Particles in Abrasive Water Jet and Acceleration Mechanism," paper E2, 9th International Symposium on Jet Cutting Technology, Sendai, Japan, Oct, 1988, pp. 217 - 238.)
Today’s topic therefore is about optimizing the abrasive feed rate into an abrasive waterjet cutting system, but you should remember that different manufacturers have different nozzle assembly designs. Thus the graphs and tables that I will use to illustrate the discussion relate to one particular nozzle design that was used at that time. Not all the nozzle designs were the same, but the results illustrate the points that I am going to make. But it underlies the recommendation that you should each run some standard tests with your system so that you have a baseline of performance and data to tell you where your system works best.
There are several reasons why different designs produce different cutting results, and I will point out some of them in what follows. To begin, however, consider again the basic elements of the waterjet mixing chamber.
Figure 1. Section through the mixing chamber of a conventional abrasive injection system.
A small high pressure stream of water enters the chamber through the upper nozzle, passes through the chamber, creating a vacuum that pulls abrasive into the chamber, and mixes with that abrasive before the resulting AWJ exits through the focusing tube.
One of the first things to understand is that, in the cutting jet that issues from the tube the actual cutting comes from the abrasive particles. From work that has been carried out at a number of places we know that the higher the velocity of the particles, the greater the damage that they will do on the target.
Figure 2. Relative mass loss when steel balls hit a mild steel plate (after Hutchings, I.M., Winter, R.E., Field, J.E., "Solid Particle Erosion of Metals;The Removal of Surface Material by Spherical Projectiles," Proceedings of the Royal Society, London, Vol. A348, 1976, pp. 379 - 392.)
Discussion in earlier posts pointed out that there are different ways in which waterjets attack ductile and brittle materials. However the relationship between an increase in impact velocity and damage occurs whether the targets are brittle or ductile. In figure 2 the target was a ductile steel, in more brittle material it is the coalescence of cracks that removes material, and higher velocities create larger cracks, as shown in figure 3.
Figure 3. Effect of impact velocity on crack length, (after Evans, A.G., "Impact Damage Mechanics: Solid Projectiles," in Erosion, Treatise on Materials Science and Technology, Vol. 16, ed C. Preece, Academic Press, 1979.).
And the same form holds true if steel balls are fired into sandstone.
Figure 4. Relative amount of Berea sandstone removed by the impact of steel balls of varying size (after Ripkin, J.F., Wetzel, J.M., A Study of the Fragmentation of Rock byImpingement with Water and Solid Impactors, Final Report on U.S. Bureau of Mines, Contract HO 210021, February, 1972.).
The above graphs show that it is more effective to have the abrasive moving faster in terms of the damage done by individual particles. Which brings up the first consideration in the design and use of an AWJ mixing chamber.
In order to get the particles moving as fast as possible they have to get their energy from the water jet entering the chamber. But the jet enters the chamber as a solid stream that then breaks into droplets (as shown in earlier pictures) as it passes down the chamber. If the jet remains in a solid stream all the way down, and out of the focusing tube, then the abrasive will find it difficult to penetrate into the center of the jet stream and pick up all the needed jet energy.
This can be illustrated by looking at the velocity and distribution of particles coming out of a nozzle with two different sizes of waterjet orifice but the same size of focusing tube diameter.
Figure 5. Relative particle distribution across a 40,000 psi jet with a focusing tube diameter of 2.3 mm (0.09 inches), and an AFR of 1 lb/min for two waterjet orifice sizes (after Mazurkiewicz, M., Olko, P., Jordan, R., "Abrasive Particle Distribution in a High Pressure Hydroabrasive Jet," International Water Jet Symposium, Beijing, China, September, 1987, pp. 4-1 - 4-10.)
The smaller waterjet breaks up fully within the chamber entraining and accelerating the abrasive particles and providing the desired cutting stream. The larger sized jet does not completely breakup, and fewer particles can mix into the center of the jet giving a more diffuse and less efficient cutting stream. In this case changing from a 0.005 inch waterjet orifice to a 0.013 inch diameter orifice (at roughly 7 times more power, because of the higher flow rate) produces a poorer result.
It is therefore important to ensure that there is an efficient energy transfer between the water and the particles. But the jet energy can only be diffused to a certain number of particles before it significantly begins to reduce in the amount of energy that it imparts to each particle. In other words if you put too much abrasive into the jet stream, then the amount of energy each particle gets is reduced, as it the overall cutting efficiency.
In an example I have used in class I noted that if I pick up a small child and run down the corridor, then I can carry the child at about my normal running speed, on the other hand if I pick up a couple of football players and try the same run I will be barely able to stagger. So the optimum carrying capacity of any jet can be determined for a given water flow rate, which is itself based on the waterjet orifice diameter and the pressure at which the water is supplied.
I will return to this topic next time, but you can see, in the concluding figure, that when a lower abrasive feed rate is fed to the nozzle, that the percentage of the abrasive moving in the higher velocity range rises to over 60% compared with only 20% of the particles when the abrasive feed is too high. And that means that the cutting performance will be less with the higher abrasive feed rates. (The numbers are a little high to reinforce the point).
Figure 7. Particle velocity distribution on leaving the focusing tube (after Isobe, T., Yoshida, H., Nishi, K., "Distribution of Abrasive Particles in Abrasive Water Jet and Acceleration Mechanism," paper E2, 9th International Symposium on Jet Cutting Technology, Sendai, Japan, Oct, 1988, pp. 217 - 238.)
Read more!
Labels:
abrasive cutting,
abrasive particles,
abrasive waterjet,
AFR
Thursday, September 12, 2013
Waterjetting 13b - Milling without a Mask
As abrasive waterjets have developed they have been used to both cut through materials, and, in more recent work, have been used to mill pockets within the internal part of the piece.
Figure 1. Milled Pocket in Glass
In the early parts of pocket milling simple linear cuts were made adjacent to one another across the space where the pocket needed to be created. However, with the need to slow the head down and reverse direction, the edges of the pocket were being cut deeper than the inside floor, and this could cause some problems with part life and utility.
The first step to overcome this problem was to provide a mask, cut to the size of the pocket to be cut, but made out of a harder material, such as steel. By placing the mask over the piece, and setting the machine so that the cuts were made at constant speed over the pocket, a flat floor could be cut. All the slowing and reversing of the head takes place over the mask, so that it is destroyed fairly quickly. But if it survives one milling, then for some parts this provides a process that cannot be achieved in other ways.
Consider, for example, the sheet of glass cut in figure 1. The corners of the pockets are relatively sharp and of consistent radius all the way down the wall, which is relatively straight. A conventional mechanical milling tool transmits high levels of force between the part being milled and tool holder. Therefore, to prevent vibrations, the tool diameter must be no less than a quarter of the tool length. This means that the radius of the pocket wall cannot be less than one-eighth of the pocket depth. That restriction does not exist with an abrasive waterjet milled pocket, where the radius can be much tighter.
This is a critical issue in the milling of parts, where the milling is to get weight out of the component. In many parts that are made for the aircraft industry the part can be designed so that much of the internal volume is not needed for strength, and can be removed to lower the weight. But with conventional tools there are limits to how much can come from a single pocket, not with the AWJ system.
As the above figure shows, and masking and other techniques allow, the radius of the corner can fall below a tenth of an inch even when milling pockets more than eight-inches deep.
There remain, however, a number of problems with the use of the masking technique. It takes time to make and install the mask, and it costs an additional expense that makes the process less competitive. One of the problems that arise with the use of masking comes with rebound of the abrasive from the mask. Dr. Hashish has illustrated this problem with a diagram.
Figure 2. Abrasive rebound from a worn mask (Dr. Hashish)
If the mask is not shaped properly, or if it has been used before and is worn, then it may have a chamfered edge. When the abrasive waterjet stream strikes the curved surface it can be reflected back onto the work piece, giving an unwanted erosion shadow along the edge of the pocket.
Another problem can arise if the speed of the nozzle, and the distance that the nozzle moves between passes is not controlled to ensure a smooth and even cut over the pocket surface. As mentioned in an earlier post, the roughness of the cut increases if the abrasive particles are allowed to bounce and make a second cut within the piece. To ensure quality, as a result, the nozzle should be moved, relatively quickly, over the workpiece.
Yet the inertia of the cutting head, and the drive assembly in the table motion controller make this difficult to do at relatively high speed. John Shepherd at PIW Corp came up with an answer to this problem, that coincidentally did away with masking.
Figure 3. The Wobbler showing the nozzle motion.
The concept behind the device is that, by slightly oribiting the motion of the focusing tube around an axis, the jet will sweep out a circular path on the workpiece. Because it is only the end of the focusing tube that is moving the forces involved are small, and easily provided through a small motor on the device. The relative speed with which the nozzle moves over the surface is now much higher, while the speed of the main arm remains relatively low. The device was studied at MS& T and the parameters that controlled the depth and quality of cut were found by Dr. Shijin Zhang as part of his doctoral research.
As with the control of single passes of a non-oscillating nozzle, the distance between adjacent passes is critical to the satisfactory performance. If the distance is too great then ridges will be generated in the floor that are almost impossibly to remove using abrasive waterjets alone. Dr. Hashish, in an early paper on milling, for example, showed that if the upper layers of a pocket are aggressively milled with higher pressures and larger grit sizes, that this floor roughness cannot be later removed by using finer grit sizes. This is because the finer grit, while removing some surface asperities will still erode the surface relatively evenly, so that the roughness pattern shown in figure 4, cannot be later removed entirely.
Figure 4. Rough floor to the pocket where the distance between adjacent passes is too great. (Dr. Zhang)
On the other hand it is not always necessary to have a high quality surface for the pocket. For example MS&T have made a number of plaques where metal plates, cut and lettered with the AWJ are then inset into pockets in polished samples of marble or granite. Since these are not strength-bearing, and the plates are glued in place, the pocket floor does not have to be of that high a quality.
Figure 5. Milled pocket in the shape of the United States, Note the edge sharpness and the narrow cutting radii.
On the other hand, where a smooth surface is required then this can be equally well achieved through programming the path of the overall head movement, so that the nozzle sweeps the floor evenly. The glass plate in Figure 1 was also milled with the Wobbler.
Figure 6. Pocket cut into metal without a mask, using the Wobbler. Note the smooth floor.
I will come back to this topic next time.
Figure 1. Milled Pocket in Glass
In the early parts of pocket milling simple linear cuts were made adjacent to one another across the space where the pocket needed to be created. However, with the need to slow the head down and reverse direction, the edges of the pocket were being cut deeper than the inside floor, and this could cause some problems with part life and utility.
The first step to overcome this problem was to provide a mask, cut to the size of the pocket to be cut, but made out of a harder material, such as steel. By placing the mask over the piece, and setting the machine so that the cuts were made at constant speed over the pocket, a flat floor could be cut. All the slowing and reversing of the head takes place over the mask, so that it is destroyed fairly quickly. But if it survives one milling, then for some parts this provides a process that cannot be achieved in other ways.
Consider, for example, the sheet of glass cut in figure 1. The corners of the pockets are relatively sharp and of consistent radius all the way down the wall, which is relatively straight. A conventional mechanical milling tool transmits high levels of force between the part being milled and tool holder. Therefore, to prevent vibrations, the tool diameter must be no less than a quarter of the tool length. This means that the radius of the pocket wall cannot be less than one-eighth of the pocket depth. That restriction does not exist with an abrasive waterjet milled pocket, where the radius can be much tighter.
This is a critical issue in the milling of parts, where the milling is to get weight out of the component. In many parts that are made for the aircraft industry the part can be designed so that much of the internal volume is not needed for strength, and can be removed to lower the weight. But with conventional tools there are limits to how much can come from a single pocket, not with the AWJ system.
As the above figure shows, and masking and other techniques allow, the radius of the corner can fall below a tenth of an inch even when milling pockets more than eight-inches deep.
There remain, however, a number of problems with the use of the masking technique. It takes time to make and install the mask, and it costs an additional expense that makes the process less competitive. One of the problems that arise with the use of masking comes with rebound of the abrasive from the mask. Dr. Hashish has illustrated this problem with a diagram.
Figure 2. Abrasive rebound from a worn mask (Dr. Hashish)
If the mask is not shaped properly, or if it has been used before and is worn, then it may have a chamfered edge. When the abrasive waterjet stream strikes the curved surface it can be reflected back onto the work piece, giving an unwanted erosion shadow along the edge of the pocket.
Another problem can arise if the speed of the nozzle, and the distance that the nozzle moves between passes is not controlled to ensure a smooth and even cut over the pocket surface. As mentioned in an earlier post, the roughness of the cut increases if the abrasive particles are allowed to bounce and make a second cut within the piece. To ensure quality, as a result, the nozzle should be moved, relatively quickly, over the workpiece.
Yet the inertia of the cutting head, and the drive assembly in the table motion controller make this difficult to do at relatively high speed. John Shepherd at PIW Corp came up with an answer to this problem, that coincidentally did away with masking.
Figure 3. The Wobbler showing the nozzle motion.
The concept behind the device is that, by slightly oribiting the motion of the focusing tube around an axis, the jet will sweep out a circular path on the workpiece. Because it is only the end of the focusing tube that is moving the forces involved are small, and easily provided through a small motor on the device. The relative speed with which the nozzle moves over the surface is now much higher, while the speed of the main arm remains relatively low. The device was studied at MS& T and the parameters that controlled the depth and quality of cut were found by Dr. Shijin Zhang as part of his doctoral research.
As with the control of single passes of a non-oscillating nozzle, the distance between adjacent passes is critical to the satisfactory performance. If the distance is too great then ridges will be generated in the floor that are almost impossibly to remove using abrasive waterjets alone. Dr. Hashish, in an early paper on milling, for example, showed that if the upper layers of a pocket are aggressively milled with higher pressures and larger grit sizes, that this floor roughness cannot be later removed by using finer grit sizes. This is because the finer grit, while removing some surface asperities will still erode the surface relatively evenly, so that the roughness pattern shown in figure 4, cannot be later removed entirely.
Figure 4. Rough floor to the pocket where the distance between adjacent passes is too great. (Dr. Zhang)
On the other hand it is not always necessary to have a high quality surface for the pocket. For example MS&T have made a number of plaques where metal plates, cut and lettered with the AWJ are then inset into pockets in polished samples of marble or granite. Since these are not strength-bearing, and the plates are glued in place, the pocket floor does not have to be of that high a quality.
Figure 5. Milled pocket in the shape of the United States, Note the edge sharpness and the narrow cutting radii.
On the other hand, where a smooth surface is required then this can be equally well achieved through programming the path of the overall head movement, so that the nozzle sweeps the floor evenly. The glass plate in Figure 1 was also milled with the Wobbler.
Figure 6. Pocket cut into metal without a mask, using the Wobbler. Note the smooth floor.
I will come back to this topic next time.
Read more!
Labels:
abrasive cutting,
abrasive particles,
glass cutting,
masking,
milling,
Wobbler
Saturday, August 3, 2013
Waterjetting 11d - AWJ and cut taper
I have spent some time in recent weeks discussing the use of abrasives in waterjet cutting, and particularly some of the issues that are involved in getting the abrasive distributed relatively evenly through the jet stream, and accelerated to as high a velocity as possible by the time the jet leaves the focusing tube.
This issue has become more important as clients request more precise cuts, and edge quality and alignment become more critical. As the jet cuts along a surface the amount of material that is removed (i.e. the depth of cut simplistically) is controlled by the number of particles that impact along that axis. And that, to a degree, is controlled by where that axis lies, relative to the axial diameter of the jet that runs parallel to the direction of cut. Different conditions give different particle densities, but even within those conditions, the material under the center of the jet will see many more particle impacts than those on the side.
Figure 1. Particle distribution across two abrasive waterjet streams with the same focusing tube diameter, but different waterjet orifice diameters (Mazurkiewicz, M., Olko, P., Jordan, R., "Abrasive Particle Distribution in a High Pressure Hydroabrasive Jet," International Water Jet Symposium, Beijing, China, September, 1987, pp. 4-1 - 4-10.)
As the above figure shows, in order to achieve the best abrasive cutting the rate of abrasive feed must be tailored to the nozzle size and the jet parameters. The density of the abrasive in the resulting stream can be optimized for those conditions and, as discussed in earlier posts, adding too much abrasive to the system will end up being counter productive.
A simple example can show this, in a test where we cut grooves in a block of granite, with the concentration of abrasive in the jet stream increasing with each pass.
Figure 2. Cuts made into a granite block, with abrasive feed rate increased as the cuts progressed from the left-side of the block to the right. Note that beyond a certain AFR the depth of cut begins to decrease. (Yazici, Sina, Abrasive Jet Cutting and Drilling of Rock, Ph.D. Dissertation in Mining Engineering, University of Missouri- Rolla, Rolla, Missouri, 1989, 203 pages.)
There is, however, a second consequence to the concentration of particles across the jet, and that is that the material under the jet on either side of the center-line of the cut will see a smaller number of particles impacting the surface, than that at the center. As a result the material will not be cut as deeply, and as the slots shown in Figure 2 illustrate, the cut will, as a result taper in on both sides.
In many applications, where the material to be cut is relatively thin, or where the exact alignment of the edge is not that critical this may not be important. However there are applications where edge alignment is required on the order of a thousandth of an inch or two over the part thickness, with the part being half-an-inch or more thick.
One way to achieve that precision of cut is to slow the traverse speed down. If the jet is moving slowly enough then there will be enough particles hitting the material at the edge of the cut, that the edge will be cut vertically downwards.
Figure 3. The effect of traverse speed on the edge taper angle (in degrees) in cutting titanium.
Notice that, because the jet tends to flare out a little as it moves away from the nozzle, the taper angle goes negative if the speed falls to too low a value. In this particular case the nozzle was moving across the surface at a speed of about quarter-of-an-inch per minute.
To get enough particles on the sides of the jet to cut a parallel slot edge, however, means that much of the abrasive in the center of the jet is not doing any work, but is rather being powered up and paid for to no real advantage. Thus, in most cases, (though not all) cutting very slowly to achieve precision on the residual edge of the cut is an overly expensive way of achieving the precision.
Given the relatively small angle that the taper cuts it is usually more cost-effective (providing the table allows this) to slightly tilt the cutting head, so that at higher cutting speeds the taper is effectively removed on the edge that is left. Obviously the taper on the piece of material being removed is made worse, but if that removed piece is going to be cut later into a different shape for another purpose, then this excessive taper on the initial surface comes with no great cost.
The taper angle and the speed relationship will vary both for the material being cut, as well as for the different parameters of the abrasive waterjet, and so – as with most cases where this sort of precision is required – a small test program to establish the best parameters for the cut will be needed.
There are other ways of achieving this precision in cutting. One is to make multiple passes over the surface, with the jet removing only very small increments of material at one time. Again if this is carried out carefully and precisely the edge quality can be maintained, at the same time as the depth of cut can be well controlled allowing pockets of material to be removed from the work piece.
However that gets into the whole issue of milling material from a target, and that is the topic for another day. It brings up the inter-relationship between traverse speed and depth of cut (which combine to give the area of cut surface, which can be used in some cases to optimize the cutting performance of a system, particularly where edge quality is not that rigid a requirement). And more particularly it brings up the quality of the walls and floor of the pockets created.
Figure 4. Factors to be considered in milling a pocket, illustrated by a multi-level pocket created in glass.
This issue has become more important as clients request more precise cuts, and edge quality and alignment become more critical. As the jet cuts along a surface the amount of material that is removed (i.e. the depth of cut simplistically) is controlled by the number of particles that impact along that axis. And that, to a degree, is controlled by where that axis lies, relative to the axial diameter of the jet that runs parallel to the direction of cut. Different conditions give different particle densities, but even within those conditions, the material under the center of the jet will see many more particle impacts than those on the side.
Figure 1. Particle distribution across two abrasive waterjet streams with the same focusing tube diameter, but different waterjet orifice diameters (Mazurkiewicz, M., Olko, P., Jordan, R., "Abrasive Particle Distribution in a High Pressure Hydroabrasive Jet," International Water Jet Symposium, Beijing, China, September, 1987, pp. 4-1 - 4-10.)
As the above figure shows, in order to achieve the best abrasive cutting the rate of abrasive feed must be tailored to the nozzle size and the jet parameters. The density of the abrasive in the resulting stream can be optimized for those conditions and, as discussed in earlier posts, adding too much abrasive to the system will end up being counter productive.
A simple example can show this, in a test where we cut grooves in a block of granite, with the concentration of abrasive in the jet stream increasing with each pass.
Figure 2. Cuts made into a granite block, with abrasive feed rate increased as the cuts progressed from the left-side of the block to the right. Note that beyond a certain AFR the depth of cut begins to decrease. (Yazici, Sina, Abrasive Jet Cutting and Drilling of Rock, Ph.D. Dissertation in Mining Engineering, University of Missouri- Rolla, Rolla, Missouri, 1989, 203 pages.)
There is, however, a second consequence to the concentration of particles across the jet, and that is that the material under the jet on either side of the center-line of the cut will see a smaller number of particles impacting the surface, than that at the center. As a result the material will not be cut as deeply, and as the slots shown in Figure 2 illustrate, the cut will, as a result taper in on both sides.
In many applications, where the material to be cut is relatively thin, or where the exact alignment of the edge is not that critical this may not be important. However there are applications where edge alignment is required on the order of a thousandth of an inch or two over the part thickness, with the part being half-an-inch or more thick.
One way to achieve that precision of cut is to slow the traverse speed down. If the jet is moving slowly enough then there will be enough particles hitting the material at the edge of the cut, that the edge will be cut vertically downwards.
Figure 3. The effect of traverse speed on the edge taper angle (in degrees) in cutting titanium.
Notice that, because the jet tends to flare out a little as it moves away from the nozzle, the taper angle goes negative if the speed falls to too low a value. In this particular case the nozzle was moving across the surface at a speed of about quarter-of-an-inch per minute.
To get enough particles on the sides of the jet to cut a parallel slot edge, however, means that much of the abrasive in the center of the jet is not doing any work, but is rather being powered up and paid for to no real advantage. Thus, in most cases, (though not all) cutting very slowly to achieve precision on the residual edge of the cut is an overly expensive way of achieving the precision.
Given the relatively small angle that the taper cuts it is usually more cost-effective (providing the table allows this) to slightly tilt the cutting head, so that at higher cutting speeds the taper is effectively removed on the edge that is left. Obviously the taper on the piece of material being removed is made worse, but if that removed piece is going to be cut later into a different shape for another purpose, then this excessive taper on the initial surface comes with no great cost.
The taper angle and the speed relationship will vary both for the material being cut, as well as for the different parameters of the abrasive waterjet, and so – as with most cases where this sort of precision is required – a small test program to establish the best parameters for the cut will be needed.
There are other ways of achieving this precision in cutting. One is to make multiple passes over the surface, with the jet removing only very small increments of material at one time. Again if this is carried out carefully and precisely the edge quality can be maintained, at the same time as the depth of cut can be well controlled allowing pockets of material to be removed from the work piece.
However that gets into the whole issue of milling material from a target, and that is the topic for another day. It brings up the inter-relationship between traverse speed and depth of cut (which combine to give the area of cut surface, which can be used in some cases to optimize the cutting performance of a system, particularly where edge quality is not that rigid a requirement). And more particularly it brings up the quality of the walls and floor of the pockets created.
Figure 4. Factors to be considered in milling a pocket, illustrated by a multi-level pocket created in glass.
Read more!
Thursday, August 1, 2013
Waterjetting 11c - Mixing abrasive with a water jet
Sometimes I would get the feeling (particularly when talking to some of my students) that the mixing chamber of an abrasive waterjet (AWJ) cutting system, together with the feeds in and the focusing nozzle outlet, were considered to be some magical black box out of which a perfect cutting stream issues to cut the desired material.
There are, in fact a variety of different chamber designs that can be purchased from different manufacturers. Some will tell you that all designs cut roughly the same, and that there is little difference between them. As I commented in one of the earliest posts in this series this is not true. Over the years we have run numerous comparative tests on different designs, using different abrasives, abrasive feed rates and target materials, and have found a broad range of results. For example, in cutting steel at a fixed traverse speed and other conditions, we found an average comparative performance as follows:
Figure 1. Comparative performance between 12 nominally similar abrasive waterjet cutting nozzles in cutting through steel at a standard speed, pump pressure, and abrasive concentration.
I described the actual test in another post, and it is clear from these averaged results that there is a wide difference in performance between the nominally similar tools.
While I don’t think there is a lot of interest in going through the details of different designs it might be helpful to explain some of the factors that play a part in producing jets of greater or lesser performance.
To return, first, to the basic construction of the mixing chamber and focusing tube assembly (AWJ nozzle), one starts by recognizing that the major cutting performance will be achieved by the particles which remove material when they hit the target. The energy that they have, however, comes from the water that is fed into the AWJ nozzle through a small jeweled orifice, or waterjet nozzle, at the top of the mixing chamber.
Figure 2. Basic nozzle design
That waterjet stream is small and initially highly focused and fast moving. As it moves through the mixing chamber, as I have described in other posts, the outer edges of the jet slow down, and gradually the jet fans out and breaks up into fragments.
There is no benefit in trying to inject the abrasive into the jet at the beginning of this passage, since, at that point, the outer layers of the jet have enough energy to knock away the particles before they can enter the fastest moving segment in the core. Rather it is better to inject the abrasive further down the chamber, so that the jet will have begun to break down into slugs, and the abrasive can be positioned so that it is impacted by a sequence of the individual slugs and accelerated to the desired velocity.
There is an additional benefit to moving the abrasive feed line a little further down the chamber. When the jet stream is rapidly switched on and off, when for example, piercing a series of small holes in a part, then the driving pressure pushing water out of the waterjet orifice switches off and on. When it switches off there is a short period where the differential pressure will draw fluid from the chamber back through the waterjet nozzle. If there are small particles of abrasive in the vicinity (and with some designs there are) then these can be drawn back through the upper orifice, and then pushed back down by the succeeding water flow in the next pulse. This can rapidly erode softer jeweled orifices, so that they round or chip, not always evenly, and degrade the resulting waterjet as it flows into the chamber. This disruption can move the jet from being in the center of the chamber, and cause poor abrasive pick-up or accelerate wear of the chamber walls, and in the focusing tube. All of these degrade performance. (The solution, if you can achieve it, is to use a diamond upper orifice, since this is largely non-responsive to the passage of the abrasive back and forth, and retains its shape and the jet performance it was designed to produce much longer – providing a cost benefit to the change).
Fig 3. Wear on a ruby waterjet orifice inserted at the top of a mixing chamber after 15 minutes of use. (The dark particles are small particles of garnet)
Figure 4. Chipping on the edges of sapphire and ruby orifices (after Powell 2007 WJTA Conference)
Fig 5. Lack of wear on a diamond insert nozzle after being in use for several hundred hours.
With the abrasive inlet channel and jet passage designed to get the abrasive into the jet where the water jet is broken up, yet still moving at high speed, there needs to be a sufficient distance for an optimal energy transfer to occur. Beyond that point, with the particle and the abrasive (which will have partially been broken in the contact between the jet and the particle, between particles striking one another, and between contact between the particle and the walls of the AWJ nozzle) the cutting jet has to be refocused into the narrow cutting stream that is required to give the finished cut surface desired.
The refocusing of the mixed jet (air, water and abrasive) is achieved with a focusing tube, which is made up of a conic section which brings the jet back together, and then a straight section which allows further energy transfer between the three component parts of the jet, before the jet issues from the orifice aimed at the target.
The passage of the particle down this tube is not always straight. Wear typically begins at the tip of the conic section as it feeds into the tube. The wear within the tube will often take up a pattern, as any irregularity in the flow causes it to bounce from one wall of the tube to the other creating a wear pattern along the walls that has a wave-like structure.
Figure 6. Wear at different points along the focusing tube
When this wear reaches the mouth of the focusing tube, then the downstream orifice is eroded out of a circular shape, and the jet that comes out no longer will cut cleanly, or to as great a depth. At that point the nozzle is worn out and should be replaced. The point at which that replacement occurs varies depending on the quality of the cut that is required. Obviously when the cut being made is at a precision of a thousandth of an inch over a cut depth of half-an-inch (as with some aircraft parts) the replacement point is reached a little earlier than if the cuts being made are a rough cut merely, for example, to separate two parts one from another, and provide a rough shape to the piece.
I’ll continue this topic in the next segment of this section.
There are, in fact a variety of different chamber designs that can be purchased from different manufacturers. Some will tell you that all designs cut roughly the same, and that there is little difference between them. As I commented in one of the earliest posts in this series this is not true. Over the years we have run numerous comparative tests on different designs, using different abrasives, abrasive feed rates and target materials, and have found a broad range of results. For example, in cutting steel at a fixed traverse speed and other conditions, we found an average comparative performance as follows:
Figure 1. Comparative performance between 12 nominally similar abrasive waterjet cutting nozzles in cutting through steel at a standard speed, pump pressure, and abrasive concentration.
I described the actual test in another post, and it is clear from these averaged results that there is a wide difference in performance between the nominally similar tools.
While I don’t think there is a lot of interest in going through the details of different designs it might be helpful to explain some of the factors that play a part in producing jets of greater or lesser performance.
To return, first, to the basic construction of the mixing chamber and focusing tube assembly (AWJ nozzle), one starts by recognizing that the major cutting performance will be achieved by the particles which remove material when they hit the target. The energy that they have, however, comes from the water that is fed into the AWJ nozzle through a small jeweled orifice, or waterjet nozzle, at the top of the mixing chamber.
Figure 2. Basic nozzle design
That waterjet stream is small and initially highly focused and fast moving. As it moves through the mixing chamber, as I have described in other posts, the outer edges of the jet slow down, and gradually the jet fans out and breaks up into fragments.
There is no benefit in trying to inject the abrasive into the jet at the beginning of this passage, since, at that point, the outer layers of the jet have enough energy to knock away the particles before they can enter the fastest moving segment in the core. Rather it is better to inject the abrasive further down the chamber, so that the jet will have begun to break down into slugs, and the abrasive can be positioned so that it is impacted by a sequence of the individual slugs and accelerated to the desired velocity.
There is an additional benefit to moving the abrasive feed line a little further down the chamber. When the jet stream is rapidly switched on and off, when for example, piercing a series of small holes in a part, then the driving pressure pushing water out of the waterjet orifice switches off and on. When it switches off there is a short period where the differential pressure will draw fluid from the chamber back through the waterjet nozzle. If there are small particles of abrasive in the vicinity (and with some designs there are) then these can be drawn back through the upper orifice, and then pushed back down by the succeeding water flow in the next pulse. This can rapidly erode softer jeweled orifices, so that they round or chip, not always evenly, and degrade the resulting waterjet as it flows into the chamber. This disruption can move the jet from being in the center of the chamber, and cause poor abrasive pick-up or accelerate wear of the chamber walls, and in the focusing tube. All of these degrade performance. (The solution, if you can achieve it, is to use a diamond upper orifice, since this is largely non-responsive to the passage of the abrasive back and forth, and retains its shape and the jet performance it was designed to produce much longer – providing a cost benefit to the change).
Fig 3. Wear on a ruby waterjet orifice inserted at the top of a mixing chamber after 15 minutes of use. (The dark particles are small particles of garnet)
Figure 4. Chipping on the edges of sapphire and ruby orifices (after Powell 2007 WJTA Conference)
Fig 5. Lack of wear on a diamond insert nozzle after being in use for several hundred hours.
With the abrasive inlet channel and jet passage designed to get the abrasive into the jet where the water jet is broken up, yet still moving at high speed, there needs to be a sufficient distance for an optimal energy transfer to occur. Beyond that point, with the particle and the abrasive (which will have partially been broken in the contact between the jet and the particle, between particles striking one another, and between contact between the particle and the walls of the AWJ nozzle) the cutting jet has to be refocused into the narrow cutting stream that is required to give the finished cut surface desired.
The refocusing of the mixed jet (air, water and abrasive) is achieved with a focusing tube, which is made up of a conic section which brings the jet back together, and then a straight section which allows further energy transfer between the three component parts of the jet, before the jet issues from the orifice aimed at the target.
The passage of the particle down this tube is not always straight. Wear typically begins at the tip of the conic section as it feeds into the tube. The wear within the tube will often take up a pattern, as any irregularity in the flow causes it to bounce from one wall of the tube to the other creating a wear pattern along the walls that has a wave-like structure.
Figure 6. Wear at different points along the focusing tube
When this wear reaches the mouth of the focusing tube, then the downstream orifice is eroded out of a circular shape, and the jet that comes out no longer will cut cleanly, or to as great a depth. At that point the nozzle is worn out and should be replaced. The point at which that replacement occurs varies depending on the quality of the cut that is required. Obviously when the cut being made is at a precision of a thousandth of an inch over a cut depth of half-an-inch (as with some aircraft parts) the replacement point is reached a little earlier than if the cuts being made are a rough cut merely, for example, to separate two parts one from another, and provide a rough shape to the piece.
I’ll continue this topic in the next segment of this section.
Read more!
Saturday, June 29, 2013
Waterjetting 10d - Abrasive sizing
Over the past 30 years abrasive waterjet cutting has become an increasingly useful tool for cutting a wide range of materials, of varying thickness and strength. However, as the range of applications for the tool has grown, so the requirements for improved performance have also risen. Before being able to make a better quality cut there had to be a better understanding of how abrasive waterjet cutting works, so that the improvements could be made.
Figure 1. Some factors that affect the cutting performance of an abrasive waterjet (After Mazurkiewicz)
This understanding has not been easy to develop, since there are many different factors that all affect how well the cutting process takes place. Consider, first of all, the process of getting the abrasive up to the fastest speed possible. And for the purpose of discussion I am going to use a “generic” mixing chamber and focusing tube nozzle for the following discussion.
Figure 2. Simplified sketch of a mixing chamber and focusing tube nozzle used in adding abrasive to a high pressure waterjet.
As high-pressure water flows through the small orifice (which in the sketch was historically made of sapphire) it enters a larger mixing chamber and creates a suction that will pull abrasive into the mixing chamber through the side passage. That side passage is connected, through a tube, to a form of abrasive feed mechanism, that I will not discuss in detail today.
However the abrasive does not flow into the mixing chamber by itself. Rather it is transported into the mixing chamber using a fluid carrier. In the some of the earliest models of abrasive waterjet systems water was used as the carrier fluid to bring the abrasive into the mixing chamber. This, as a general rule, turned out to be a mistake.
The problem is that, within the mixing chamber, the energy that comes into the chamber with the high-pressure water has to mix, not only with the abrasive, but also with the fluid that carried the abrasive into the chamber. Water is heavier than air, and so if water is the carrier fluid, then it will absorb more of the energy that is available, with the result that there is less for the abrasive, which – as a result – does not move as quickly and therefore does not cut as well. The principle was first discussed by John Griffiths at the 2nd U.S. Waterjet Conference, although he was discussing abrasive use in cleaning at the time.
Figure 3 Difference in performance of water acting to carry the abrasive to the mixing chamber (wet feed) in contrast with the use of air as the carrier fluid. (Griffiths, J.J., "Abrasive Injection Usage in the United Kingdom," 2nd U.S. Waterjet Conference, May, 1983, Rolla, MO, pp. 423 - 432.)
Note that this is not the same as directly mixing the abrasive into the waterjet stream under pressure – abrasive slurry jetting – which I will discuss in later posts.
The difference between the two ways of bringing the abrasive to the mixing chamber is clear enough that almost from the beginning only air has been considered as the carrier to bring the abrasive into the mixing chamber. However there is the question as to how much air is enough, how much abrasive should be added, and how effectively the mixing process takes place.
In the earlier developments the equipment available restricted the range of pressures and flow rates at which the high pressure water could be supplied, and these limits bounded early work on the subject.
One early observation, however, was that the size of the abrasive that was being fed into the mixing chamber was not the average size of the abrasive after cutting was over. (At that time steel was not normally used as a cutting abrasive). Because the fracture of the abrasive into smaller pieces might mean that the cutting process became less effective, Greg Galecki and Marian Mazurkiewicz began to measure particle sizes, at different points in the process. (Galecki, G., Mazurkiewicz, M., Jordan, R., "Abrasive Grain Disintegration Effect During Jet Injection," International Water Jet Symposium,Beijing, China, September, 1987, pp. 4-71 - 4-77.)
For example, by firing the abrasive-laden jet along the axis of a larger plastic tube (here opened to show the construction) the abrasive would, after leaving the nozzle, decelerate and settle into the bottom of the tube, without further break-up, and without damage to the tube. Among other results this allowed a measure of how fast the particles leave the nozzle, since the faster they were moving, then the further they would carry down the pipe.
Figure 4. Test to examine particle size and travel distance, after leaving the AWJ nozzle at the left of the picture. The containing tube has divisions every foot, and small holes over blue containers, so that the amount caught in every foot could be collected and measured.
For one particular test the abrasive going into the system was carefully screened to be lie in the size range between 170 and 210 microns. It was then fed into a 30,000 psi waterjet at a feed rate of 0.6 lb/minute. The particles were captured, after passing through the mixing chamber, but before they could cut anything, by using the tube shown in Figure 4. The size of the particles was then measured, and plotted as a cumulative percentage adding the percentages found at each sieve size over the range to the 210 micron size of the starting particles.
Figure 5. Average size of particles after passing through a mixing chamber and exiting into a capture tube, without further damaging impact.
The horizontal line shows the point where 50% of the abrasive (by weight) had accumulated, and the vertical line shows that this is at a particle size of 140 microns. Thus, just in the mixing process alone energy is lost in mixing the very fast moving water, with the initially much slower moving abrasive.
And, as an aside, this is where the proper choice of abrasive becomes an important part of an effective cutting operation. Because the distribution of the curve shown in figure 5 will change, with abrasive type, size, concentration added, as well as the pressure and flow rate of the nozzle through which the water enters the mixing chamber.
I will have more to discuss on this in the next post, but will leave you with the following result. After we had run the tests which I just mentioned, we collected the abrasive in the different size ranges. Then we used those different size ranges to see how well the abrasive cut. This was one of the results that we found.
Figure 6. The effect of the size of the feed particles into the abrasive cutting system on the depth of cut which the AWJ achieved.
You will note that down to a size of around 100 microns the particle size did not make any significant difference, but that once the particle size falls below that range, then the cutting performance degrades considerably. (And if you go back to figure 5, you will note that about 30% of the abrasive fell into that size range, after the jet had left the mixing chamber).
Figure 1. Some factors that affect the cutting performance of an abrasive waterjet (After Mazurkiewicz)
This understanding has not been easy to develop, since there are many different factors that all affect how well the cutting process takes place. Consider, first of all, the process of getting the abrasive up to the fastest speed possible. And for the purpose of discussion I am going to use a “generic” mixing chamber and focusing tube nozzle for the following discussion.
Figure 2. Simplified sketch of a mixing chamber and focusing tube nozzle used in adding abrasive to a high pressure waterjet.
As high-pressure water flows through the small orifice (which in the sketch was historically made of sapphire) it enters a larger mixing chamber and creates a suction that will pull abrasive into the mixing chamber through the side passage. That side passage is connected, through a tube, to a form of abrasive feed mechanism, that I will not discuss in detail today.
However the abrasive does not flow into the mixing chamber by itself. Rather it is transported into the mixing chamber using a fluid carrier. In the some of the earliest models of abrasive waterjet systems water was used as the carrier fluid to bring the abrasive into the mixing chamber. This, as a general rule, turned out to be a mistake.
The problem is that, within the mixing chamber, the energy that comes into the chamber with the high-pressure water has to mix, not only with the abrasive, but also with the fluid that carried the abrasive into the chamber. Water is heavier than air, and so if water is the carrier fluid, then it will absorb more of the energy that is available, with the result that there is less for the abrasive, which – as a result – does not move as quickly and therefore does not cut as well. The principle was first discussed by John Griffiths at the 2nd U.S. Waterjet Conference, although he was discussing abrasive use in cleaning at the time.
Figure 3 Difference in performance of water acting to carry the abrasive to the mixing chamber (wet feed) in contrast with the use of air as the carrier fluid. (Griffiths, J.J., "Abrasive Injection Usage in the United Kingdom," 2nd U.S. Waterjet Conference, May, 1983, Rolla, MO, pp. 423 - 432.)
Note that this is not the same as directly mixing the abrasive into the waterjet stream under pressure – abrasive slurry jetting – which I will discuss in later posts.
The difference between the two ways of bringing the abrasive to the mixing chamber is clear enough that almost from the beginning only air has been considered as the carrier to bring the abrasive into the mixing chamber. However there is the question as to how much air is enough, how much abrasive should be added, and how effectively the mixing process takes place.
In the earlier developments the equipment available restricted the range of pressures and flow rates at which the high pressure water could be supplied, and these limits bounded early work on the subject.
One early observation, however, was that the size of the abrasive that was being fed into the mixing chamber was not the average size of the abrasive after cutting was over. (At that time steel was not normally used as a cutting abrasive). Because the fracture of the abrasive into smaller pieces might mean that the cutting process became less effective, Greg Galecki and Marian Mazurkiewicz began to measure particle sizes, at different points in the process. (Galecki, G., Mazurkiewicz, M., Jordan, R., "Abrasive Grain Disintegration Effect During Jet Injection," International Water Jet Symposium,Beijing, China, September, 1987, pp. 4-71 - 4-77.)
For example, by firing the abrasive-laden jet along the axis of a larger plastic tube (here opened to show the construction) the abrasive would, after leaving the nozzle, decelerate and settle into the bottom of the tube, without further break-up, and without damage to the tube. Among other results this allowed a measure of how fast the particles leave the nozzle, since the faster they were moving, then the further they would carry down the pipe.
Figure 4. Test to examine particle size and travel distance, after leaving the AWJ nozzle at the left of the picture. The containing tube has divisions every foot, and small holes over blue containers, so that the amount caught in every foot could be collected and measured.
For one particular test the abrasive going into the system was carefully screened to be lie in the size range between 170 and 210 microns. It was then fed into a 30,000 psi waterjet at a feed rate of 0.6 lb/minute. The particles were captured, after passing through the mixing chamber, but before they could cut anything, by using the tube shown in Figure 4. The size of the particles was then measured, and plotted as a cumulative percentage adding the percentages found at each sieve size over the range to the 210 micron size of the starting particles.
Figure 5. Average size of particles after passing through a mixing chamber and exiting into a capture tube, without further damaging impact.
The horizontal line shows the point where 50% of the abrasive (by weight) had accumulated, and the vertical line shows that this is at a particle size of 140 microns. Thus, just in the mixing process alone energy is lost in mixing the very fast moving water, with the initially much slower moving abrasive.
And, as an aside, this is where the proper choice of abrasive becomes an important part of an effective cutting operation. Because the distribution of the curve shown in figure 5 will change, with abrasive type, size, concentration added, as well as the pressure and flow rate of the nozzle through which the water enters the mixing chamber.
I will have more to discuss on this in the next post, but will leave you with the following result. After we had run the tests which I just mentioned, we collected the abrasive in the different size ranges. Then we used those different size ranges to see how well the abrasive cut. This was one of the results that we found.
Figure 6. The effect of the size of the feed particles into the abrasive cutting system on the depth of cut which the AWJ achieved.
You will note that down to a size of around 100 microns the particle size did not make any significant difference, but that once the particle size falls below that range, then the cutting performance degrades considerably. (And if you go back to figure 5, you will note that about 30% of the abrasive fell into that size range, after the jet had left the mixing chamber).
Read more!
Wednesday, June 19, 2013
Waterjetting 10c - Abrasive waterjet cutting
There are a number of different abrasives that can be supplied by different sources, and the market for the small grains that are used in abrasive waterjet cutting extends considerably beyond just the waterjet business. All abrasives are not created equal, some work better in one condition, others in another. As with other tools that the waterjet cutter or cleaner will use, first you should decide what the need for the abrasive is, and run a small series of tests to find out which is the best set of cutting conditions for that particular job.
The first item on the list should be the material that has to be cut. (Although abrasives are also used in cleaning, that will be covered in a later post). There are, simplifying greatly, two classes of material that have to be cut. One class responds in a brittle way (think glass) and the other responds in a ductile or yielding manner (think metal). Because of these different responses, when the particles hit the surface, the way in which cuts are best made will vary between the two. Some years ago Ives and Ruff shot abrasive particles at different targets and found that there was a difference in the amount of material removed, but the best angle at which the particles should be aimed changed with the material.
Figure 1. The Effect of change in impact angle on erosion rate for ductile and brittle targets. (Ives and Ruff, Wear, 1978, pp 149 – 162).
Some work at MS&T just before I retired indicated that the shape of these curves changed a little, depending on the size of the abrasive that is used. There are also some changes with abrasive shape. And this is because of the entirely different way in which an abrasive particle cuts into the two different materials. In this post we’ll discuss only the ductile target.
If a relatively smooth particle is shot into a ductile material at an angle perpendicular to the surface, then when it hits the surface the target material will flow out from underneath, but not be removed. As the following micro-photograph shows the particles can become embedded in the material – and even add to the weight of the piece on rare occasion.
Figure 2. Microphotograph showing a sand particle buried in the surface of an aluminum target.
There is very little material removed in this case, as the black curve shows in Figure 1, when the impact angle approaches 90 degrees. Consider that if you take a knife and push it down into butter you don’t remove any butter. But if you drag the knife over the butter surface you will peel off a layer.
So it is with abrasive hitting a ductile metal. If the abrasive is brought in at an angle, (optimized in the figure at 15 degrees) then the abrasive has a cutting energy along the surface and this will peel up, and remove small pieces of the surface. By taking a microphotograph along the edge of an abrasive cut, we were able to show the action of individual particles in cutting into the metal.
Figure 3. Individual particle impacts on an aluminum surface, showing the cutting and plowing action of the particles.
Where the surface is plowed up, but not removed, another particle has to hit that point to remove the relatively fragile lip. However, if the particle is a copper slag, or other relatively weak material, it can shatter during the cutting process, and the breaking pieces can break off that lip, so that – again in the right material – the slag may give a better performance than a more expensive alternative.
But if we are to cut metal in this way, what does that say about the shape of the particles that we need to use. Obviously if they were round, such as a steel or glass shot, then there would be no sharp edges to cut into and peel off the material. Thus a steel or glass grit will cut better, though each particle needs a certain thickness in all dimensions so that there will be enough energy to both cut into the material, and plow along it.
Figure 4. Difference in cut depth achieved with broken glass fragments over glass beads when cutting metal.
A relatively round particle with sharp corners, and garnet is usually such a particle, can often work well in cutting a range of different ductile materials.
Figure 5. Schematic of how a particle of different shapes might cut into material.
Now that is fine when a high-pressure abrasive waterjet (AWJ) is starting to cut into the surface, but as the jet cuts down into the surface the angle of the cut will change. Yet even if the jet is pointing directly down into the target, and moving along to cut through it, the cut surface is not usually a straight line down through the material.
Figure 6. Cutting through glass, note the curved path of the jet through the one-inch material.
Cuts into Plexiglas and other clear materials have allowed research scientists to monitor the cut path through the target, as a function of time. It is not a constant shape, but, as Dr. Henning showed at the 18th International Conference, the edge of the cut changes with time. You can see the results of this in cuts that are made through metal where the paths of the cut, particularly lower in the cut, curve around and back towards the start of the cut.
Figure 7. Cut into steel, with the face piece of metal removed to show the cut surface.
This path confirms an explanation first proposed by Dr Lars Ohlsson in his doctorate at Lulea in Sweden. He pointed out that the change in the surface of the cut is caused by the sequence of actions that a particle sees as it comes down onto the surface.
First it comes in almost vertically, with no lateral energy, and it cuts in the smooth, upper part of the cut. Then it rebounds out of the cut, but into the jet stream that gives it a little more energy, and directs it along the cut to a second point where it will cut a little bit more of the metal. But during the first rebound the particle does not bounce perfectly along the cut, but deviates to one side or the other. This means that when it makes the second cut, it will now cut more into one side of the wall or the other. Thus, where the second bounce occurs, so the surface gets a little rougher.
Figure 8. Frames from a high speed video showing abrasive waterjet cutting of glass, with the jet cutting, rebounding down the cut and then cutting again. (Lars Ohlsson “The Theory and Practice of Abrasive Water Jet Cutting”, Doctoral Thesis, Division of Materials Processing, Lulea University of Technology, 1995)
By the time of the third cut and rebound, the jet will now be coming into the opposing side of the cut with an even greater lateral portion of its energy, and so the cut will get a little rougher. Remember also that each cut is made up of the impacts of very many particles. So that succeeding particles also rebound along the curve cut by the preceding particle, and this also will exacerbate the roughness of the cut.
We’ll talk a little about reducing this effect in the next post.
The first item on the list should be the material that has to be cut. (Although abrasives are also used in cleaning, that will be covered in a later post). There are, simplifying greatly, two classes of material that have to be cut. One class responds in a brittle way (think glass) and the other responds in a ductile or yielding manner (think metal). Because of these different responses, when the particles hit the surface, the way in which cuts are best made will vary between the two. Some years ago Ives and Ruff shot abrasive particles at different targets and found that there was a difference in the amount of material removed, but the best angle at which the particles should be aimed changed with the material.
Figure 1. The Effect of change in impact angle on erosion rate for ductile and brittle targets. (Ives and Ruff, Wear, 1978, pp 149 – 162).
Some work at MS&T just before I retired indicated that the shape of these curves changed a little, depending on the size of the abrasive that is used. There are also some changes with abrasive shape. And this is because of the entirely different way in which an abrasive particle cuts into the two different materials. In this post we’ll discuss only the ductile target.
If a relatively smooth particle is shot into a ductile material at an angle perpendicular to the surface, then when it hits the surface the target material will flow out from underneath, but not be removed. As the following micro-photograph shows the particles can become embedded in the material – and even add to the weight of the piece on rare occasion.
Figure 2. Microphotograph showing a sand particle buried in the surface of an aluminum target.
There is very little material removed in this case, as the black curve shows in Figure 1, when the impact angle approaches 90 degrees. Consider that if you take a knife and push it down into butter you don’t remove any butter. But if you drag the knife over the butter surface you will peel off a layer.
So it is with abrasive hitting a ductile metal. If the abrasive is brought in at an angle, (optimized in the figure at 15 degrees) then the abrasive has a cutting energy along the surface and this will peel up, and remove small pieces of the surface. By taking a microphotograph along the edge of an abrasive cut, we were able to show the action of individual particles in cutting into the metal.
Figure 3. Individual particle impacts on an aluminum surface, showing the cutting and plowing action of the particles.
Where the surface is plowed up, but not removed, another particle has to hit that point to remove the relatively fragile lip. However, if the particle is a copper slag, or other relatively weak material, it can shatter during the cutting process, and the breaking pieces can break off that lip, so that – again in the right material – the slag may give a better performance than a more expensive alternative.
But if we are to cut metal in this way, what does that say about the shape of the particles that we need to use. Obviously if they were round, such as a steel or glass shot, then there would be no sharp edges to cut into and peel off the material. Thus a steel or glass grit will cut better, though each particle needs a certain thickness in all dimensions so that there will be enough energy to both cut into the material, and plow along it.
Figure 4. Difference in cut depth achieved with broken glass fragments over glass beads when cutting metal.
A relatively round particle with sharp corners, and garnet is usually such a particle, can often work well in cutting a range of different ductile materials.
Figure 5. Schematic of how a particle of different shapes might cut into material.
Now that is fine when a high-pressure abrasive waterjet (AWJ) is starting to cut into the surface, but as the jet cuts down into the surface the angle of the cut will change. Yet even if the jet is pointing directly down into the target, and moving along to cut through it, the cut surface is not usually a straight line down through the material.
Figure 6. Cutting through glass, note the curved path of the jet through the one-inch material.
Cuts into Plexiglas and other clear materials have allowed research scientists to monitor the cut path through the target, as a function of time. It is not a constant shape, but, as Dr. Henning showed at the 18th International Conference, the edge of the cut changes with time. You can see the results of this in cuts that are made through metal where the paths of the cut, particularly lower in the cut, curve around and back towards the start of the cut.
Figure 7. Cut into steel, with the face piece of metal removed to show the cut surface.
This path confirms an explanation first proposed by Dr Lars Ohlsson in his doctorate at Lulea in Sweden. He pointed out that the change in the surface of the cut is caused by the sequence of actions that a particle sees as it comes down onto the surface.
First it comes in almost vertically, with no lateral energy, and it cuts in the smooth, upper part of the cut. Then it rebounds out of the cut, but into the jet stream that gives it a little more energy, and directs it along the cut to a second point where it will cut a little bit more of the metal. But during the first rebound the particle does not bounce perfectly along the cut, but deviates to one side or the other. This means that when it makes the second cut, it will now cut more into one side of the wall or the other. Thus, where the second bounce occurs, so the surface gets a little rougher.
Figure 8. Frames from a high speed video showing abrasive waterjet cutting of glass, with the jet cutting, rebounding down the cut and then cutting again. (Lars Ohlsson “The Theory and Practice of Abrasive Water Jet Cutting”, Doctoral Thesis, Division of Materials Processing, Lulea University of Technology, 1995)
By the time of the third cut and rebound, the jet will now be coming into the opposing side of the cut with an even greater lateral portion of its energy, and so the cut will get a little rougher. Remember also that each cut is made up of the impacts of very many particles. So that succeeding particles also rebound along the curve cut by the preceding particle, and this also will exacerbate the roughness of the cut.
We’ll talk a little about reducing this effect in the next post.
Read more!